Sputtering targets are the consumable source material in physical vapour deposition (PVD): energetic ions bombard the target surface and eject atoms that condense as a thin film on the substrate. For fabs, coating houses and R&D labs, the choice of target material, purity and bonding directly determines film composition, yield and cost. This guide covers how to think about those choices and what to put in a quotation request.
Purity is usually stated as 3N (99.9%), 4N (99.99%), 5N (99.999%) or higher. Higher purity reduces foreign-atom inclusions that cause arcing, pinholes and shifts in resistivity or optical bandgap. For most semiconductor and display work 4N–5N is the norm; decorative and some functional coatings can run at 3N to control cost. The right grade is a trade-off between film spec and budget, not a simple "higher is better".
Brittle ceramic or low-thermal-conductivity targets are typically indium-bonded or elastomer-bonded to a copper or aluminum backing plate so heat dissipates and the target survives the process. Specify the backing material, bonding method and whether you need a bonded assembly or the target alone. Mismatched bonding is one of the most common causes of premature target failure.
A useful request includes: material and target purity, dimensions and tolerance, bonding/backing requirement, quantity, required certification (RoHS/REACH, composition report), and the target application. Photographs of an existing spent target help suppliers match the form factor and assess recyclable material. For a quotation in English, contact our export team with drawings or photos; we supply sputtering targets and recover spent targets for recycling across Shandong Province with door collection for larger lots.
Yes. ITO and precious-metal targets in particular retain most of their contained metal and are recovered through assay-based refining; recycling offsets the cost of new target purchases.
ITO targets for displays are typically 4N indium basis with controlled Sn content; the exact grade depends on the film's resistivity and transmission spec, so share the film requirement rather than guessing a number.
Both. Bonded assemblies are supplied when the application needs a backing plate for thermal management; unbonded targets are available for customers who bond in-house.
Liaocheng Feiyan New Material Technology Co., Ltd.
Address: Room 8-1503, 15F, Building 9, Xingguang International Financial Center, Dongchang East Road, Dongcheng Sub-district, Liaocheng Economic and Technological Development Area, Shandong, China
Tel: 0635-2112001 / 19963594228 | Email: fykj425@gmail.com
Copyright © Liaocheng Feiyan New Material Technology Co., Ltd.. All Rights Reserved.